MİNERAL KATKILARIN YÜKSEK DAYANIMLI KENDİLİĞİNDEN YERLEŞEN HARÇ ÖZELLİKLERİNE ETKİLERİ

تحميل...
thumbnail.project.alt
المساهمين
الممولين
رقم التعريف
238
الباحث
Mohammed Miftah Abdullah BEEDIQ
المشرفين
منشورات
وحدات تنظيمية
الوصف
compressive and flexural strengths of the laboratory and steam cured samples were tested, and the water absorption, ultrasound transmission rate, and BHA values of the 90-day samples were determined. Slag, RHA, and slag-RHA substitution had a negative effect on the early age strength, but steam curing created significant strength increases in the mechanical strength of the 28-day samples. In both curing conditions, 40% slag-30% RHA substitution resulted in a significant increase in 90-day mechanical strengths. It has been observed that 2% PVA fiber additive affects the strengths positively.
الكلمات الدالة
KEYWORDS: Self-compacting concrete, Ground granulated blast furnace slag, Rice husk ash, PVA fiber, Mechanical properties